- Abrasion Wear Resistance
- ASTM D-4060, CS-17 tested. Between 0.08 gm - 0.1 gm max weight loss depending on version of Stonclad
- Compression
- ASTM C-579 tested. Between 11,500 psi - 5,000 psi depending on version of Stonclad.
- Flammability
- ASTM E-648 tested. Class 1
- Flexural Strength
- ASTM C-580 tested. Between 5,000 psi - 2,000 psi depending on version of Stonclad.
- Hardness
- ASTM D-2240, Shore D tested. Result between 80 to 90
- Light Blocking
- Complete
- Maintenance
- For regular maintenance, use Stonkleen D2G with a mop and bucket or an automatic floor scrubbing machine. Deep cleaning for healthcare environments may require diluted Stonkleen AS9 to remove sanitizing and disinfecting films and residues that are left behind from health code protocols that, over time, will leave heavy build-up and dull the floor. Refer to manufacturer's documentation for additional information
- Performance
- Has a cure rate of 8 hours for foot traffic and 24 hours for normal operations
- Tensile Strength
- ASTM C-307 tested. Between 2,200 psi - 1,000 psi depending on version of Stonclad
- Water Absorption
- ASTM E-648 tested. Result <1%