Pre-casted. Engineered from Portland cement with reclaimed fly ash and recycled marble & granite chips. Poured into a mold and vacuum-packed with vibro-compaction
6.90 Mpa; ASTM C-120 Modulus of rupture Tested. Dry result of 1,800 psi. Wet result of 800 psi
Light Blocking
Complete
Maintenance
To maintain surface luster, apply standard cleaning methods and use neutral detergents. Avoid cleaning products that contain acid (even when diluted), alkaline detergents, strong solvents and paint strippers. Cleaning can be simply done by wet mopping with a neutral detergent; then rinse thoroughly with clean water and let dry
Tensile Strength
ASTM D-209 Tested. Dry result of 600 psi. Wet result of 450 psi